When the 110 wt c steel is cooled under equilibrium


When the 1.10 wt% C steel is cooled under equilibrium conditions from 925 (deg C),

(i) what are the relative amounts of the primary or proeutectoid phase, the pearlite, and the total ferrite phase immediately below the eutectoid temperature at 726 (deg C)? and

(ii) what is the weight fraction of pearlite at 400 (deg C)