Nickel containing 2 wt thorium is produced in powder form


Nickel containing 2 wt% thorium is produced in powder form, consolidated into a part, and sintered in the presence of oxygen, causing all of the thorium to produce ThO2 spheres 80 nm in diameter. Calculate the number of spheres per cm3. (Note: The density of ThO2 is 9.86 g/cm3.)