Estimate the time required to achieve the concentration


For a steel alloy it has been determined that a carburizing heat treatment of 25 hours duration will increase the carbon concentration to 0.55 wt% at a point of 3.0mm from the surface. Estimate the time required to achieve the same concentration at a position 6.0mm from the surface for an identical steel and at the same carburizing temperature.

Request for Solution File

Ask an Expert for Answer!!
Mechanical Engineering: Estimate the time required to achieve the concentration
Reference No:- TGS0842096

Expected delivery within 24 Hours